Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 258 °F | ASTM D648 |
RheTech Products GC20P255-00 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural Applications: Underhood componentsElectrical housingsHeadlamp bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 258 °F | Annealed; ASTM D648 |
M. Holland Company PC522R Polycarbonate High flowHigh impact resistanceGood mold releaseApplications: AppliancesFood containersTable products |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 258 °F | Unannealed, 0.125 in; ASTM D648 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 258 °F | unannealed; ASTM D648 |
Styron CALIBREâ„¢ 2061-22 Polycarbonate CALIBREâ„¢ 2061-22 resin is used in applications involving steam or ethylene oxide for sterilization - though suitability for use in these applications is dependent upon autoclave cycle times and.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 258 °F | 0.157 in, unannealed; ASTM D648 |
Styron EMERGEâ„¢ 4310-22 Polycarbonate EMERGEâ„¢ PC 4310-22 advanced resin is high-performance polycarbonate resin offering high heat resistance, toughness, and superior flow. Applications: Consumer Electronics and Information Techn.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 258 °F | 0.157 in, unannealed; ASTM D648 |
Styron EMERGEâ„¢ 4330-22 Polycarbonate EMERGEâ„¢ PC 4330-22 advanced resin is high-performance polycarbonate resin offering ultraviolet light stability, high heat resistance, toughness, and superior flow. Applications: Consumer Elec.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 258 °F | Unannealed, 0.125 in; ASTM D648 |
Styron CALIBREâ„¢ 301 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 258 °F | Unannealed, 0.125 in; ASTM D648 |
Styron CALIBREâ„¢ 303 EP Polycarbonate Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 258 °F | Unannealed; ASTM D648 |
Chase Plastics CP Pryme® AH300 Acetal Homopolymer, Recycled Content Features: General purposeHigh heat resistanceGood chemical resistanceGood dimensional stabilityFatigue resistantLow frictionGrease resistantLow moisture absorptionOil resistantHigh rigiditySolvent r.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 126 °C | 258 °F | ASTM D648 |
RheTech Products GC20P255-712UV 20% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, B231 Earth Grey Applications: Consumer goodsMiscellaneous bracketsExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |