Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 245 °F | ASTM D648 |
RheTech Products GC35P200-01UV 35% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, General Purpose Black Applications: BracketsStructural componentsHeadlamp housingsWindow frameInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 245 °F | ASTM D648 |
Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled PC/ABS Alloy, General Purpose, 20% Glass FilledProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 245 °F | ASTM D648 |
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 245 °F | ASTM D648 |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 245 °F | ASTM D648 |
Polymer Resources PC-IM3 Polycarbonate, Impact Modified, High Flow Polycarbonate, Impact Modified, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 245 °F | ASTM D648 |
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 245 °F | ASTM D648 |
Polymer Resources TP-FR IM2 PBT, Impact Modified, Flame Retardant, High Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 245 °F | ASTM D648 |
Polymer Resources TP-FR-IM2 Polybutylene Terephthalate, Impact Modified, Flame Retardant, High Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 245 °F | ASTM D648 |
Polymer Resources TP-FR-IM2-[color]-6 Polybutylene Terephthalate, Low Temperature Impact Modified, Flame Retardant Polybutylene Terephthalate, Low Temperature Impact Modified, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 245 °F | unannealed, .125in; ASTM D648 |
Star Plastics PC/PET7901 Molding Grade PC/PET Information provided by Star Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 245 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/ABS 8800 Availability: North AmericaForms: PelletsFeatures: High Impact Resistance and High Temperature StrengthProcessing Method: Profile ExtrusionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 - 124 °C | 245 - 255 °F | ASTM D648 |
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice.. |