Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 220 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D-648
Plaskolite Optix® CA - 87 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D-648
Plaskolite Optix® CP - 86 General Purpose Acrylic Resin
OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli..
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
Unannealed; ASTM D648
Oxford Polymers ABS 30GF-BK ABS, 30% Glass Fiber Reinforced
Product Description: Glass Fiber (30% Reinforced), ABS injection molding grade Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: Pre-colo..
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D648
Quadrant EPP Fluorosint® 135 PTFE and PPS Blend, with Proprietary Lubrication Fillers (ASTM Product Data Sheet)
Chemical resistance parallels PTFE Continuous use temperatures to 500°F (260°C) Compared to PTFE higher load carrying capability 1/9 of the deformation under load lower coefficient of thermal exp..
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D648
Polymer Resources AC-GP2-TFE5 Acetal Copolymer, 5% PTFE
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D648
Polymer Resources PPX-MF-FR3 Modified-PPO, V-0 Flame Retardant, Mineral Reinforced
Modified-Polyphenylene Oxide, V-0 Flame Retardant, 230F HDT, Mineral ReinforcedFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mecha..
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D-648
Plaskolite West Optix® CP - 86 UVA General Purpose Acrylic Resin
Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av..
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
Unannealed, 0.125 in bars; ASTM D648
PolyOne Lubri-Tech™ AT-000/8T Acetal-Copolymer, PTFE Lubricated  (discontinued **)
Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation.
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
Unannealed; ASTM D648
Techmer ES Electrablend® ABS CF10 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
Unannealed; ASTM D648
Techmer ES Electrablend® ABS CF25 BK 25% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 25% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6/6 04003 Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizedAppearance: Natu..
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6/6 ML2 HS NAT Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Molybdenum Disulfide Lubricant(2%)Features: Lubricated, Good Wear Resistance, Low Friction and Heat StabilizerAppear..
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
Unannealed; ASTM D648
Techmer ES Luriblend® PA6/6 ML2 Nylon 66
Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Good Wear ResistanceInformation provided by TP Composites, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D648
Techmer ES Plaslube® AC-81/TF/15 NAT Acetal (POM) Homopolymer
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
Unannealed; ASTM D648
Chase Plastics CP Pryme® A130 ABS, 30% Glass Fiber Reinforced
Features: Glass fiber reinforcementInjection moldingForm: PelletsInformation provided by Chase Plastics.
Deflection Temperature at 1.8 MPa (264 psi) 104 - 120 °C
220 - 248 °F
Average value: 112 °C Grade Count:6
Overview of materials for PC/ABS + Stainless Steel
This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro..
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
220 °F
ASTM D648
Polymer Resources PPX-MF-FR3 Modified PPO, UL 94 V-0 with HDT of 230 F, Mineral Reinforced  (Unverified Da
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.