Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.3 °C

@Thickness 6.35 mm
191 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne Edgetek® XT XT-500-CU00 Polycarbonate + PBT (PC+PBT)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Deflection Temperature at 1.8 MPa (264 psi) 88.3 °C

@Thickness 6.35 mm
191 °F

@Thickness 0.250 in
Annealed; ASTM D648
PolyOne Edgetek® XT XT-500-CX02 PC+PBT  (discontinued **)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Deflection Temperature at 1.8 MPa (264 psi) 88.3 °C
191 °F
Annealed; ASTM D648
American Polymers API 500 Polystyrene
API 500 is a heat resistant grade of impact polystyrene. It has superior heat resistance, good impact resistance and easy colorability.Applications: API 500 is used in housewares, toys, containers,..
Deflection Temperature at 1.8 MPa (264 psi) 88.3 °C
191 °F
0.125 in bar Unannealed/Conditioned 48 hours at 23°C; ASTM D648
Diamond Polymers ABS 4001HH
Description: Heat Resistant Grade, High HeatInformation provided by Diamond Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 88.3 °C
191 °F
Unannealed; ASTM D648
Entec Hyrene® PSCRY 2.5 General Purpose Polystyrene
Available in North America Features: Crystal, General Purpose, and High Heat ResistanceRoHS Compliant Form: Pellets Information provided by Entec
Deflection Temperature at 1.8 MPa (264 psi) 88.3 °C
191 °F
ASTM D-648
Axiall HHW-191 Rigid PVC, Extrusion
Georgia Gulf HHW-191 is a special purpose profile extrusion alloy designed for applications requiring the following properties: Excellent WeatherabilityImpact Strength & ToughnessColorabilityChemic..
Deflection Temperature at 1.8 MPa (264 psi) 88.3 °C
191 °F
ASTM D648
Americas Styrenics MB3150 High Heat Crystal Polystyrene
Product CharacteristicsFast cycling due to high heat distortion temperatureHigh vicat softening temperatureExcellent clarity with slight blue tintGood toughnessFood Contact CompliantUL Classificatio..
Deflection Temperature at 1.8 MPa (264 psi) 88.3 °C
191 °F
ASTM D648
Americas Styrenics STYRON® 610 High Heat Crystal Polystyrene
Product CharacteristicsAdditive freeTypical ApplicationsFoamsFilms/opticalCarrier resinSpecialty blendingInformation provided by AmericasStyrenics LLC.
Deflection Temperature at 1.8 MPa (264 psi) 88.3 °C

@Thickness 6.35 mm
191 °F

@Thickness 0.250 in
Annealed; ASTM D648