Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 186 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
Unannealed; 104°C (219°F) annealed; ASTM Data
Dow Isoplast® 151 Polyurethane (PUR-RT), Impact Modified  (discontinued **)
ISOPLAST® 151 resin is an impact modified amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include excellent chemical resistance, high heat, low mois..
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
0.250 in; ASTM D648
M. Holland Company AB105 ABS
Features: Medium Flow, High Impact Resistance, Good StiffnessUses: Household Goods, Packaging Processing Method: Injection MoldingInformation provided by M. Holland.
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
ASTM D648
Chevron Phillips EA3400 Medium Flow Crystal
DescriptionChevron EA3400 is a medium flow-crystal polystyrene resin developed to blend with Styrene-Butadiene block copolymers for sheet extrusion and vacuum thermoforming. EA3400 can be used in c..
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
Unannealed; ASTM D648
Entec Hyrene® PS-HI 8/2 High Impact Polystyrene
Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
Unannealed; ASTM D648
Entec Hyril® GP355AS Styrene Acrylonitrile
Available in North America Features: Copolymer Automotive Specifications: DELPHI M-9565-9 Color: Blue-TransparentForm: PelletsProcessing Method: ExtrusionInformation provided by Entec
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
Unannealed; ASTM D648
Entec Hyrene® PS-HI 3/2 High Impact Polystyrene
Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
Unannealed; ASTM D648
Entec Hyril® SAN500 Styrene Acrylonitrile
Available in North America Features: Copolymer Form: PelletsInformation provided by Entec
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
ASTM D648
Diapolyacrylate Acrypet® IR H70 Impact Modified PMMA
Acrypet® is a registered trade mark of Diapolyacrylate Company Limited. Information provided by Dayson Polymers.
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
ASTM D648
Americas Styrenics STYRON A-TECH® 1290 High Impact Polystyrene
Product CharacteristicsEasy processingGood impact resistanceESCRFood Contact CompliantUL Classification 94HBTypical ApplicationsCreamer and yot containersExtrusion/ thermoformingInformation provided..
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
ASTM D648
Americas Styrenics STYRON® 668 High Heat Crystal Polystyrene
Product CharacteristicsHigh heatGood balance of flow and toughnessFood Contact CompliantUL Classification 94HBTypical ApplicationsDisposable cutleryCD and DVD jewel boxesInformation provided by Amer..
Deflection Temperature at 1.8 MPa (264 psi) 85.6 °C
186 °F
Unannealed; ASTM Data
Americas Styrenics Styron® 612 Polystyrene  (discontinued **)
STYRON® 612 general purpose polystyrene resin is an easy flow resin with no color additives. When used unmodified for the manufacture of food contact articles STYRON 612 complies with the US Food, ..
Copyright © lookpolymers.com All Rights Reserved