Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 83.3 °C | 182 °F | ASTM D-648 |
Plaskolite Optix® CP - 924 High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.3 °C | 182 °F | ASTM D-648 |
Plaskolite West Optix® CP - 924 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.3 °C | 182 °F | Unannealed; 101°C (214°F) annealed; ASTM Data |
Americas Styrenics Styron® 685 Polystyrene
(discontinued **) STYRON® 685 general purpose polystyrene resin is a high heat resin used in consumer electronics and housewares. It offers excellent clarity, good moldability for use in hot runner systems. When use.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 83.3 °C | 182 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 685P Polystyrene
(discontinued **) STYRON® 685P general purpose polystyrene resin is a high heat resin with good strength, moldability/processability, and excellent clarity. This resin is typically used in consumer electronic applic.. |