Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 81.7 °C | 179 °F | Unannealed; ASTM Data |
Americas Styrenics Styron® 613 Polystyrene
(discontinued **) STYRON® 613 high heat, high strength general purpose polystyrene is typically used in applications requiring a clear, tough part such as office products and magnetic media enclosures. It offers goo.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.7 °C | 179 °F | Unannealed; ASTM D648 |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.7 °C | 179 °F | Unannealed; ASTM D648 |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.7 °C | 179 °F | ASTM D648 |
Cast Nylons Nycast® GX Solid Lubricant Filled Gray Cast Nylon 6 NYCAST® GX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 81.7 °C | 179 °F | ASTM D648 |
Cast Nylons Nycast® RX Solid Lubricant Filled Red Cast Nylon 6 NYCAST® RX is a specially formulated, self-lubricating grade designed to deliver low coefficient of friction, superior wear resistance, high pressure/velocity performance, and low moisture absorpti.. |