Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 170 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.7 - 170 °C
170 - 338 °F
Average value: 110 °C Grade Count:49
Overview of materials for Polyphenylene Ether, Heat Resistant
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Heat Resistant". Each property range of values reported is minimum and maximum valu..
Deflection Temperature at 1.8 MPa (264 psi) 140 - 170 °C
284 - 338 °F
Injection; ISO 75-A
Raschig Group RALUPOL® 8601 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic moulding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical stren..
Deflection Temperature at 1.8 MPa (264 psi) 140 - 170 °C
284 - 338 °F
Injection; ISO 75-A
Raschig Group RALUPOL® 8602 UP
Glass-fiber reinforced polyester molding compound. Mold shrinkage similar to phenolic molding compounds, low post-shrinkage, good electrical values, excellent heat resistance, good mechanical streng..
Deflection Temperature at 1.8 MPa (264 psi) 65.0 - 170 °C
149 - 338 °F
Average value: 100 °C Grade Count:3
Overview of materials for Nylon 12, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr..
Deflection Temperature at 1.8 MPa (264 psi) 47.0 - 170 °C
117 - 338 °F
Average value: 101 °C Grade Count:7
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..
Deflection Temperature at 1.8 MPa (264 psi) 150 - 170 °C
302 - 338 °F
ISO 75 Af
Vyncolit 3520 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..