Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 120 - 143 °C | 248 - 289 °F | Average value: 130 °C Grade Count:38 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 - 143 °C | 125 - 290 °F | Average value: 132 °C Grade Count:45 |
Overview of materials for Polycarbonate, Stainless Steel Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 104 - 143 °C | 220 - 290 °F | Average value: 120 °C Grade Count:7 |
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 75.0 - 143 °C | 167 - 290 °F | Average value: 130 °C Grade Count:59 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |