Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 115 - 124 °C | 239 - 255 °F | Average value: 120 °C Grade Count:8 |
Overview of materials for Glass Reinforced, Modified SMA This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 118 - 124 °C | 245 - 255 °F | ASTM D648 |
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon Offering improved tensile, compressive and flexural properties over conventional unfilled cast nylon, NYCAST® GF (Glass Filled)-30% provides increased load bearing characteristics and is the choice.. |