Deflection Temperature at 1.8 MPa (264 psi) 102 - 110 °C
215 - 230 °F
Average value: 106 °C Grade Count:7
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Deflection Temperature at 1.8 MPa (264 psi) 51.7 - 110 °C
125 - 230 °F
Average value: 74.1 °C Grade Count:52
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Deflection Temperature at 1.8 MPa (264 psi) 104 - 110 °C
219 - 230 °F
ASTM D648
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Deflection Temperature at 1.8 MPa (264 psi) 80.0 - 110 °C
176 - 230 °F
GB/1634
Zhejiang Juner PC/PBT Alloy
Applications: Shell of Small Household Electric Appliance, Auto Electric Appliance PartsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Deflection Temperature at 1.8 MPa (264 psi) 80.0 - 110 °C
176 - 230 °F
GB/1634
Zhejiang Juner PC/PET Alloy
Applications: Shell of Small Household Electric Appliance, Auto Electric Appliance PartsInformation provided by Zhejiang Juner New Materials Co, Ltd.
Deflection Temperature at 1.8 MPa (264 psi) 47.8 - 110 °C
118 - 230 °F
Average value: 60.4 °C Grade Count:34