Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | ASTM D648 |
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | ASTM D648 |
RheTech Products FT4600-152 Thermoplastic Polyolefin, UV Stabilized, JA6A Black Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | ASTM D648 |
RheTech Products P252-01 Polypropylene Copolymer, Black Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | ASTM D648 |
RheTech Products P256-01A Polypropylene Copolymer, Black Applications: Lower IP componentsUnderhood clipsGlove box binInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | ASTM D648 |
RheTech Products P257-00 Polypropylene Copolymer, Natural Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | ASTM D648 |
RheTech Products P257-01 Polypropylene Copolymer, Black Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 - 110 °C | 125 - 230 °F | Average value: 74.1 °C Grade Count:52 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | Unannealed; ASTM D648 |
M. Holland Company CP300 Polypropylene Copolymer Features: Medium Flow, High Impact Resistance, Good StiffnessUses: Appliances, Business, Equipment, Tool/Tote Box, ToysApprovals: FDA 21 CFR 177.1520 Processing Method: Injection MoldingInformatio.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6 IM 811 HS L (Dry) Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedTPCI# 6109102Information provided by TP Comp.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6 IM HS L BK Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUL File Number: E157318Processing Method: In.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PA6 IM L Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | Unannealed; ASTM D648 |
Techmer ES Elastoblend® PBT E IM SL3 Availability: North AmericaForms: PelletsAdditive: Impact Modifier and Silicone LubricantFeatures: Impact Modified and LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | ASTM D648 |
Spartech PE4130 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | ASTM D648 |
Spartech PE4325 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | ASTM D648 |
Spartech PP7120 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PBT 613 RD Availability: North AmericaForms: PelletsUL File Number: E157318Appearance: Red8661111Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PBT E Availability: North AmericaForms: PelletsFeatures: High ViscosityProcessing Method: Extrusion and Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP 0123 C Polypropylene Availability: North AmericaForms: PelletsFeatures: Copolymer and Thermally ConductiveInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PA6/ABS 1120 B1 Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® PP CO FR-N V2 Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | ASTM D648 |
Chase Plastics CP Pryme® N100STL (DAM) Nylon 6, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | annealed; ASTM D648 |
Arkema Group Solarkote® P-610 Acrylic PVC Capstock, clear, low glossInformation provided by Arkema Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | annealed; ASTM D648 |
Arkema Group Solarkote® P-601 Acrylic PVC Capstock, white, high glossInformation provided by Arkema Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 51.7 °C | 125 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® PP CO 99074 Availability: North AmericaForms: PelletsFeature: Copolymer and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc. |