Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 8.0 MPa | 195 - 235 °C | 383 - 455 °F | Average value: 219 °C Grade Count:9 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Deflection Temperature at 8.0 MPa | 195 °C | 383 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® TSG-60 PA666-GF60 Product description: Grilon TSG-60 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 60% glass fibers. Grilon TSG-60 has the following important properties: Very high st.. |
|||
Deflection Temperature at 8.0 MPa | 195 °C | 383 °F | HDT/C; ISO 75-2 |
Akro-Plastic Akromid® T1 GF 40 9 (3499) PPA Dry, 40% Glass Filled The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high.. |