Thermal Properties Metric English Comments
Deflection Temperature at 8.0 MPa 185 °C
365 °F
ISO 75-2
Hexion Bakelite™ PF 4109 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, low shrinkage, high mechanical strength, U..
Deflection Temperature at 8.0 MPa 185 °C
365 °F
ISO 75-1,-2
Lanxess Durethan® AKV 30 H3.0 000000 Nylon 66, 30% Glass Fibers
PA 66, 30% glass fibers, injection molding, heat-ageing stabilized
Deflection Temperature at 8.0 MPa 185 °C
365 °F
ISO 75-1/-2
Lanxess Durethan® AKV 35 H2.0 901510 Nylon 66, 35% Glass Fiber
PA 66, injection molding grade, 35% glass fibers, good heat-ageing resistanceApplication Examples: gearbox oil sumps, oil modules
Deflection Temperature at 8.0 MPa 185 °C
365 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVS-5H nat PA*-GF50
Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide..
Deflection Temperature at 8.0 MPa 185 °C
365 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSC-20/4 EC black 9832 PA666-CF20
Information provided by EMS Grivory
Deflection Temperature at 8.0 MPa 185 °C
365 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSC-30/4 EC black 9832 PA666-CF30
Product description: Grilon TSC-30/4 EC is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% carbon fibers. Grilon TSC-30/4 EC has the following important properties:El..
Deflection Temperature at 8.0 MPa 185 °C
365 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSC-40/4 EC black 9832 PA666-CF40
Information provided by EMS Grivory
Deflection Temperature at 8.0 MPa 185 °C
365 °F
ISO 75-1/-2
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50
Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
Deflection Temperature at 8.0 MPa 185 °C
365 °F
HDT/C; ISO 75-2
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Deflection Temperature at 8.0 MPa 185 °C
365 °F
ISO 75-2
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,..
Copyright © lookpolymers.com All Rights Reserved