Thermal Properties Metric English Comments
Brittleness Temperature -14.0 °C
6.80 °F
Wide variability between samples is observed.; ASTM D746
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Carbon Black Filled Compound  (d
Carbon black compound with 100 parts Hypalon; 27.8 parts sublimed litharge dispersion; 55 parts carbon black; 55 parts aromatic process oil; 0.5 parts MTBS; and 2 parts Tetrone® A rubber accelerato..
Brittleness Temperature -14.0 °C
6.80 °F
ASTM D746-79
DuPont Performance Polymers Hypalon® 48 Chlorosulfonated Polyethylene Rubber, Mineral Filled Compound  (discon
Mineral filled compound with 100 parts Hypalon; 80 parts hard clay; 4 parts magnesia; 30 parts aromatic process oil; 3 parts pentaerythritol; and 2 parts Tetrone® A rubber accelerator (from DuPont ..
Brittleness Temperature -14.0 °C
6.80 °F
ASTM D746
Chevron Phillips Marlex® 1409 Injection Molding Resin  (discontinued **)
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 111, A 22200Characteristics: Good Flexibility, Excellent Flow, Excellent Warping Resistance, Excellent Mold Release, Moderate ESCRApplications..
Brittleness Temperature -14.0 °C
6.80 °F
ASTM D746
Teknor Apex APEX® 80102 Polyvinyl Chloride, Flexible
Notes: 75°C Insulation; RoHS Compliant Uses: InsulationAgency Ratings: UL 1063; UL 1581; UL 62; UL 83 Forms: Pellets Wire Types: TWInformation Provided by Teknor Apex
Brittleness Temperature -14.0 °C
6.80 °F
Daikin DAI-EL G-603 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 71% Fluorine Content
Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Information provided by Daikin Industries.
Brittleness Temperature -14.0 °C
6.80 °F
ASTM D746
Alliance Polymers Zythane™ 4050D Thermoplastic Polyurethane Elastomer
Zythane™ 4050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Brittleness Temperature -14.0 °C
6.80 °F
ASTM D746
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer
Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Brittleness Temperature -14.0 °C
6.80 °F
ASTM D-746
Axiall 19871 Wire & Cable Flexible PVC
Non-lead stabilized, 105°C rated insulation compound with very good migration and oil resistance. Recommended for toner resistance applications.Information provided by Georgia GulfGeorgia Gulf bec..
Brittleness Temperature -14.0 °C
6.80 °F
ASTM D-746
Axiall 2161A Wire & Cable Flexible PVC
Flame retardant, oil resistant, 105°C rated jacket compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Brittleness Temperature -14.0 °C
6.80 °F
ASTM D746
Teknor Apex APEX® 94-A0098A-90 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I..
Brittleness Temperature -14.0 °C
6.80 °F
Sylvin Technologies 6055 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Brittleness Temperature -14.0 °C
6.80 °F
ASTM D746
PolyOne Geon™ Vinyl Wire & Cable W649LF Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide..