Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -7.78 °C | 18.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R 980A Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -7.78 °C | 18.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible R1700D Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | <= -7.78 °C | <= 18.0 °F | ASTM D746 |
CPC - Vycom POLYCARVE™ Coextruded High Density Sheet (HDPE) PolyCarve™ thermoplastic engraving sign stock made to permanently resist the destructive outdoor elements, and certain indoor environments. PolyCarve is a high density, UV stabilized polyethylene c.. |
|||
Brittleness Temperature | <= -7.78 °C | <= 18.0 °F | ASTM D746 |
CPC - Vycom SEABOARD™ GRIP-X™ Slip Resistant High Density Polyethylene (HDPE) Grip-X is a UV stabilized high density polyethylene (HDPE) sheet formulated to meet demanding conditions of the marine industry. Grip-X is manufactured with a special surface treatment and stipulate.. |