Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | <= -71.0 °C | <= -95.8 °F | ASTM D746 |
SCG Chemicals EL-Leneâ„¢ LD1902F Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactContains 1400 ppm slip content and 2400 ppm antiblocking contentRecommended Applications:G.. |
|||
Brittleness Temperature | -71.0 °C | -95.8 °F | ASTM D746 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Brittleness Temperature | -71.0 °C | -95.8 °F | ASTM D746 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Brittleness Temperature | -71.0 °C | -95.8 °F | ASTM D746 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Brittleness Temperature | -71.0 °C | -95.8 °F | ASTM D746 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Brittleness Temperature | -71.0 °C | -95.8 °F | ASTM D746 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Brittleness Temperature | -71.0 °C | -95.8 °F | ASTM D746 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Brittleness Temperature | <= -71.0 °C | <= -95.8 °F | ASTM D746 |
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Brittleness Temperature | <= -71.0 °C | <= -95.8 °F | ASTM D746 |
Chevron Phillips Marlex® 9006 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Brittleness Temperature | <= -71.0 °C | <= -95.8 °F | ASTM D746 |
Chevron Phillips Marlex® 9012 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 55600Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage ResistanceApplications:Food Pails.. |
|||
Brittleness Temperature | <= -71.0 °C | <= -95.8 °F | ASTM D746 |
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 232, A 53600Characteristics: Good Flow, Good Impact Strength, Good Stiffness, Good ESCR, Good Shrinkage ResistanceApplications:Housewares.. |
|||
Brittleness Temperature | -71.0 °C | -95.8 °F | ASTM D746 |
DuPont™ Surlyn® 9520 Ionomer Resin, Zinc Surlyn® 9520 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Brittleness Temperature | -71.0 - -70.0 °C | -95.8 - -94.0 °F | Average value: -70.2 °C Grade Count:5 |
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Rotational Molded". Each property range of values reported i.. |