Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -53.9 °C | -65.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B65T0 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -53.9 °C | -65.0 °F | ASTM D746 |
ExxonMobil Santoprene® 121-85M100 Thermoplastic Elastomer A hard, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Brittleness Temperature | -53.9 °C | -65.0 °F | ASTM D746 |
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Brittleness Temperature | -53.9 °C | -65.0 °F | ASTM D746 |
ExxonMobil Santoprene® 271-87 Thermoplastic Elastomer A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Brittleness Temperature | -53.9 °C | -65.0 °F | ASTM D746 |
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Brittleness Temperature | -53.9 °C | -65.0 °F | ASTM D746; ISO 812 |
Advanced Polymer Alloys Alcryn® 4680 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Brittleness Temperature | -53.9 °C | -65.0 °F | ASTM D746; ISO 812 |
Advanced Polymer Alloys Alcryn® 3055 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Brittleness Temperature | -53.9 °C | -65.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible A55G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |
|||
Brittleness Temperature | -53.9 °C | -65.0 °F | ASTM D746 |
ExxonMobil Santoprene® 101-87 Thermoplastic Elastomer A hard, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |