Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJAC35L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible B85UB Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
PolyOne Geon™ Vinyl Flexible XV3782 Polyvinyl Chloride, Flexible (PVC, Flexible) All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high .. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 3610-85 Polyvinyl Chloride, Flexible Uses: Medical/Healthcare Applications Agency Ratings: NSF 61 Forms: Pellets Additional Information: First Generation SeriesInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 586 Polyvinyl Chloride, Flexible Notes: 60°C Insulation; RoHS Compliant Uses: Tubing; Wire JacketingForms: Pellets Wire Types: SPT-1; SPT-2 Agency Ratings: UL 498; UL 62 Processing Method: Injection Molding Additional Informatio.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 6500-80 Polyvinyl Chloride, Flexible Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 65014 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 80328-YFR Polyvinyl Chloride, Flexible Notes: 75°C Insulation; RoHS Compliant Features: Flame Retardant; Good UV Resistance Uses: Cable Jacketing; InsulationAgency Ratings: UL QMTT2 .E73402 Forms: Pellets Wire Types: TWInformation Pro.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 85-J644Z-3 Polyvinyl Chloride, Flexible Notes: 105°C Jacket Forms: Pellets Agency Ratings: UL 13; UL 1424; UL 1655; UL 2250; UL 444 Wire Types: CATV; CL3; CMX; CL2; CM; FT-4Information Provided by Teknor Apex |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 94-A0098C-80 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-ClearForms-PelletsProcessing Method-Injection Molding.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex Flexalloy® 9300-80 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 130-P Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Features: Flame Retardant; Sunlight Resistant (720 hours) Uses: Flexible Cord Jacketing Forms: Pellets Wire Types: SJTW; STW; SVT; SRDT Agency Ratings: UL QMTT2.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 327 Polyvinyl Chloride, Flexible Notes: 60°C Insulation; RoHS Compliant Uses: Flexible Cord Insulation; Flexible Cord JacketingForms: Pellets Wire Types: SJT; SPT-1; SPT-2; SPT-3; SRDT; ST; SVT Agency Ratings: UL 1581; UL 62 Pro.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 80328 Polyvinyl Chloride, Flexible Notes: 80°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsAgency Ratings: UL QMTT2 .E73402 Forms: Pellets Wire Types: TWInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 80328-Y Polyvinyl Chloride, Flexible Notes: 75°C Insulation; RoHS Compliant Features: Sunlight Resistant (720 hours) Uses: Cable Jacketing; InsulationAgency Ratings: UL QMTT2 .E73402 Forms: Pellets Wire Types: TWInformation Provided.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | |
Sylvin Technologies 503 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | |
Sylvin Technologies 5108 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 82-E254NL-9 Polyvinyl Chloride, Flexible Notes: 80°C Jacket; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | |
Sylvin Technologies 574 PVC Wire/Cable Compound Information provided by Sylvin Technologies Inc. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | |
Colorite Polymers 8011 Clear Extrusion Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for the extrusion of various components for the production of devices. The vinyl components used in pre.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | |
Colorite Polymers 8012 Clear Injection Molding Vinyl Compound Description: Clear non-toxic vinyl compounds are utilized by the health and medical industries for injection molding of various components such as drip chambers, connectors, valves, etc. The vinyl c.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | |
Colorite Polymers Self Frosting™ 8011SF Vinyl Compound Description: Colorite has developed a family of vinyl compounds to satisfy the needs of those who need a smooth, low gloss, low friction surface for the products that they produce. Historically, thi.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D-746 |
Axiall 2134N Moldings & Extrusions Flexible PVC 105C plug molding compound. UL recognized component for 94 V-2 in all colors (0.75 mm min. thickness) and 94 V-0 in black and white (1.5 mm min. thickness). UL QMFZ2 recognized component.Informati.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D-746 |
Axiall 19470 Wire & Cable Flexible PVC Semi-rigid, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by Georgia .. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D-746 |
Axiall 19473 Wire & Cable Flexible PVC Non-lead stabilized, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 2590-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D746 |
Teknor Apex APEX® 84131 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Uses: Transportation Wire JacketingAgency Ratings: UL 62; UL QMTT2 .E73402 Forms: Pellets Wire Types: SAE; SJTW; SPT-1; SPT-2; SPT-3; SRDT; STW; SVTInformation P.. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 6510/K Flexible PVC, Lead Free Pipes, UL 94 Class V1 |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | ASTM D-746 |
Axiall 19471 Wire & Cable Flexible PVC Semi-rigid, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by Georgia .. |
|||
Brittleness Temperature | -29.0 °C | -20.2 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds PM 7075 Flexible PVC, Lead Free Various profiles |