Polymer Property : Working Point = 2300 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Working Point 1260 °C
2300 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott DURAN® Borosilicate Glass
Borosilicate glass 3.3 acc. To ISO 3585, chemically and thermally highly resistant, general-purpose glass for apparatus for the chemical industry, for pipelines, and glasswareInformation provided by..
Working Point 1260 °C
2300 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott DURATAN® Borosilicate Glass
Prestressed borosilicate glass 3.3, chemically and thermally highly resistant, Flameproof lighting The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below ..
Working Point 1260 °C
2300 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott Glass 8347 Borosilicate Glass
Borosilicate glass 3.3 acc. To ISO 3585, chemically and thermally highly resistant, highly UV-transmitting The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium i..
Working Point 1260 °C
2300 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott KIMAX® Borosilicate Glass
Laboratory Glass Drainline from Borosilicate glass 3.3. Chemically and thermally highly resistant.The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10..
Working Point 1260 °C
2300 °F
Viscosity 10<sup>4</sup> dPa s
Schott BORO-8330â„¢ Borosilicate Glass
Borosilicate glass 3.3 acc. ISO 3585, chemically highly resistant, highly resistant to thermal shock, special applications in the pharmaceutical industryInformation provided by SCHOTT AG.
Working Point 1260 °C
2300 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Schott CONTURAX® Borosilicate Glass
Borosilicate glass tubing and rod, varying types of inner and outer shapes Lighting, giftware, and decoration The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromi..