Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
UL 746 |
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-UV2-D-[color]-1 Polycarbonate, UV-stabilized, Medium Flow with Mold Release Polycarbonate, UV-stabilized, Medium Flow with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Infor.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746 |
PolyOne Bergamid™ A700 G15 HW UF Polyamide 66 (Nylon 66) These products contain flame retardants which are activated by longer residence times in the cylinder and then can decompose. At interruption of the moulding cycle (approx. >5 min) it is recommended.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746 |
PolyOne Bergamid™ A700 G20 HW UF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 6.00 mm |
248 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Crastin® LW9020FR BK851 PBT
(Unverified Data**) Crastin® LW9020FR BK851 is a 20% glass fiber reinforced, flame retardant, black polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional sta.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.750 mm |
248 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Rynite® 415HP BK503 PET
(Unverified Data**) Rynite® 415HP BK503 is a 15% glass reinforced modified polyethylene terephthalate with improved for easy, fast processing over a broad molding range with excellent balance of strength, stiffness, a.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746 |
Polymer Resources PC-UV3-D Polycarbonate, UV-stabilized, High Flow Polycarbonate, UV-stabilized, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) Zytel® 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.710 mm |
248 °F @Thickness 0.0280 in |
UL746B |
DSM Akulon® K224-HG5 (Dry) 25% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.710 mm |
248 °F @Thickness 0.0280 in |
UL746B |
DSM Akulon® K224-HG5 (Cond.) 25% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.710 mm |
248 °F @Thickness 0.0280 in |
UL746B |
DSM Akulon® K224-HG8 (Cond.) 40% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.710 mm |
248 °F @Thickness 0.0280 in |
UL746B |
DSM Akulon® K224-HG5 Nylon 6-25% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.710 mm |
248 °F @Thickness 0.0280 in |
UL746B |
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.710 mm |
248 °F @Thickness 0.0280 in |
UL746B |
DSM Akulon® K224-HG8 Nylon 6-40% Glass Reinforced (European Grade) (Dry)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness >=0.750 mm |
248 °F @Thickness >=0.0295 in |
|
LG Chemical LUPOL GP1000FC Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness >=1.50 mm |
248 °F @Thickness >=0.0591 in |
|
LG Chemical Lupox® GP2300G PBT+GF30% Description: Injection Molding, PBT+GF30%, HCFC ResistanceApplication: E&E (Muffler of Refrigerator)CAS No. 65997-17-3 and 24968-12-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness >=3.00 mm |
248 °F @Thickness >=0.118 in |
|
LG Chemical Lupox® TE5006F PET+PC Description: Injection Molding, PET+PC, Flame Retardant, GWIT, CTIApplication: IT/OA, E&E (Connector)CAS No. 68928-70-1, 103598-77-2, 25038-59-9 and 1309-64-4Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.710 mm |
248 °F @Thickness 0.0280 in |
UL746B |
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.710 mm |
248 °F @Thickness 0.0280 in |
UL746B |
DSM Akulon® K224-HG7 (Dry) 35% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.750 mm |
248 °F @Thickness 0.0295 in |
UL 746 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
UL 746 |
Ascend Performance Materials Vydyne® R530H Black Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H Black is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. It is specifically designed to maximize the retention of physical properties wh.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.830 mm |
248 °F @Thickness 0.0327 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) Zytel® FR70G25V0 NC010 is a 25% glass fiber reinforced, heat stabilized, flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.710 mm |
248 °F @Thickness 0.0280 in |
UL 746 |
Ascend Performance Materials Vydyne® R513H Nylon 66, 13% Glass Filled, Dry as Molded Vydyne® R513H is general-purpose, 13% glass-reinforced, heat stabilized PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine feed, flow, and mold .. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 0.850 mm |
248 °F @Thickness 0.0335 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 1.50 mm |
248 °F @Thickness 0.0591 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |
|||
UL RTI, Mechanical with Impact | 120 °C @Thickness 3.00 mm |
248 °F @Thickness 0.118 in |
DAM; UL 746B |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |