Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 155 °C @Thickness 0.350 mm |
311 °F @Thickness 0.0138 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 0.750 mm |
311 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 1.50 mm |
311 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 2.00 mm |
311 °F @Thickness 0.0787 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 3.00 mm |
311 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 PET
(Unverified Data**) Rynite® FR530 BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 3.00 mm |
311 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 3.00 mm |
311 °F @Thickness 0.118 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 2.00 mm |
311 °F @Thickness 0.0787 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 1.50 mm |
311 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 1.50 mm |
311 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 0.750 mm |
311 °F @Thickness 0.0295 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 2.00 mm |
311 °F @Thickness 0.0787 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 0.350 mm |
311 °F @Thickness 0.0138 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530L BK507 PET
(Unverified Data**) Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers |
|||
UL RTI, Electrical | 155 °C @Thickness 0.400 mm |
311 °F @Thickness 0.0157 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
UL RTI, Electrical | 155 °C @Thickness 0.800 mm |
311 °F @Thickness 0.0315 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
UL RTI, Electrical | 155 °C @Thickness 1.50 mm |
311 °F @Thickness 0.0591 in |
UL 746B |
DuPont Performance Polymers Rynite® FR530 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |