Thermal Properties Metric English Comments
Pour Point -9.44 °C
15.0 °F
Lubriplate 72-C Oil Food Machinery Oil
Class H-2** oil, for use as a steam peeler oil as it provides an oiliness film which prevents chatter.Available in Bottles, Jugs, Pails, 1/4 Drums and DrumsH-1 Class Lubricants are manufactured with..
Pour Point -9.44 °C
15.0 °F
Lubriplate FMO 3800 AW USP Mineral Oil-Based Food Machinery Grade Oil
For use where a Class H-1 oil is required. Manufactured in nine ISO grades for a variety of applications. Anti-wear fortified. NOTE: FMO-350AW is also available in a red and orange color which helps..
Pour Point -9.44 °C
15.0 °F
Lubriplate SPO-277 Petroleum-Based Gear, Bearing, & Recirculating Oil
Petroleum-based oils specifically designed for industrial applications such as gear cases, bearings, chains, machine ways, and general oiling. These tacky lubricants will provide anti-wear lubricati..
Pour Point -9.44 °C
15.0 °F
Dow SPECTRIM™ 35B-S Polyol
SPECTRIM™ 35B-S reaction moldable polymer is one component (SPECTRIM™ 35A is the other) of a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology dev..
Pour Point -9.44 °C
15.0 °F
Dow SPECTRIM™ 50B-S Polyol
SPECTRIM™ 50B-S reaction moldable polymer is one component (SPECTRIM™ 35B-S is the other) of a two-component polyurethane system that incorporates advanced internal mold release (IMR) technology d..
Pour Point <= -9.44 °C
<= 15.0 °F
ASTM D 97
ConocoPhillips 320 Bearing Oil
Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosi..
Pour Point <= -9.44 °C
<= 15.0 °F
ASTM D 97
ConocoPhillips 220 Bearing Oil
Description: Conoco Bearing Oil is formulated for the circulating systems that lubricate roll-neck bearings in steel and nonferrous rolling mills. It is suited for systems in which water and corrosi..