Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 362 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 362CP-2 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 363F (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 363F-WHITE (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 741E (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 744 (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 744-UV (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants NPE-UC4 Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants UniFlor 8510 (487) (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 706C (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 706CS (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 706D-UV (IG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 902 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 902B (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D97 |
Solvay Specialty Polymers FOMBLIN® M60 PFPE Lubricant Information provided by Solvay Solexis, Inc. |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D97 |
ExxonMobil Mobil Aero HFS Mobil Aero HFA, HF, and HFS are formulated for aircraft systems where use of hydrocarbon-based hydraulic fluids is required. They are low viscosity products, high VI (viscosity index) fluid with exc.. |
|||
Pour Point | -60.0 °C | -76.0 °F | |
ExxonMobil Mobil Avrex S Turbo 256 Mobil Avrex S Turbo 256 gas turbine lubricant is a combination of a highly stable synthetic base fluid and a unique chemical additive package. The combination provides outstanding thermal and oxid.. |
|||
Pour Point | -60.0 °C | -76.0 °F | |
ExxonMobil Mobil Turbo 319A-2 Mobil Turbo 319A-2 is a fully synthetic lubricant developed to meet the performance requirements of Russian gas turbine aircraft engines which operate on mineral-oil-based lubricants. Formulated fro.. |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D97 |
ExxonMobil Univis HVI 13 Exxon Univis HVI is a line of premium performance anti-wear hydraulic oils characterized by their unusually high viscosity indexes. They are engineered to maintain close viscosity control over wide .. |
|||
Pour Point | -60.0 °C | -76.0 °F | DIN ISO 3016 |
The Chemical Company VESTINOL® INB Benzoic Acid Isononyl Ester VESTINOL® INB is a new plasticizer based on benzoic acid and is not subject to any chemical classification and labeling requirements. The unique combination of low plastisol viscosity, combined wi.. |
|||
Pour Point | -60.0 °C | -76.0 °F | |
ConocoPhillips Syncon® 32 Synthetic AW Hydraulic Fluid 32 Syncon AW Hydraulic Fluid is a premium quality, synthetic antiwear hydraulic fluid developed for use in industrial and mobile equipment operating at extreme temperatures. It is particularly recommen.. |
|||
Pour Point | <= -60.0 °C | <= -76.0 °F | ASTM D5950/D97 |
ExxonMobil SpectraSyn Plus™ 4 Advanced Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn Plus™ Advanced Polyalphaolefin (PAO) provide an optimal combination of volatility and low-temperature fluidity. SpectraSyn Plus™ Advanced products viscosity indices.. |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D97 |
ExxonMobil 15 Mobil EAL Arctic Series Mobil EAL Arctic Series are high performance Environmental Awareness Lubricants (EAL) that are fully synthetic products designed specifically for the lubrication of refrigeration compressors and sys.. |
|||
Pour Point | -60.0 °C | -76.0 °F | |
ExxonMobil Mobil Avrex S Turbo 256 Mobil Avrex S Turbo 256 gas turbine lubricant is a combination of a highly stable synthetic base fluid and a unique chemical additive package. The combination provides outstanding thermal and oxid.. |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D97 |
ExxonMobil Univis HVI 13 Exxon Univis HVI is a line of premium performance anti-wear hydraulic oils characterized by their unusually high viscosity indexes. They are engineered to maintain close viscosity control over wide .. |
|||
Pour Point | -60.0 °C | -76.0 °F | ASTM D-97 |
ConocoPhillips ANDEROL® FGC 5 Fluid, Synthetic Mechanical Seal Fluid ISO 22 Description: ANDEROL FGC 5 Mechanical Seal Fluid is a synthetic hydrocarbon (PAO) based lubricant. FGC 5 Fluid meets the former H-1 approval requirements of the USDA where incidental food contact ca.. |
|||
Pour Point | -60.0 °C | -76.0 °F | Base Oil; ASTM D97 |
Nye Lubricants 783C (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -60.0 °C | -76.0 °F | |
ExxonMobil Mobil Avrex M Turbo 201/1010 Mobil Avrex M Turbo 201/1010 gas turbine lubricant is a combination of a proven aviation engine mineral oil base stock and an ashless additive package. The effective operating range for Mobil Avrex .. |