Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -36.0 °C | -32.8 °F | Base Oil; ASTM D97 |
Nye Lubricants 176 (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -36.0 °C | -32.8 °F | Base Oil; ASTM D97 |
Nye Lubricants 176A (SO) Synthetic Oil Information provided by Nye Lubricants. |
|||
Pour Point | -36.0 °C | -32.8 °F | |
ExxonMobil Mobil Clean 10W-30 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Pour Point | -36.0 °C | -32.8 °F | |
ExxonMobil Mobil Clean 10W-40 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Pour Point | -36.0 °C | -32.8 °F | ASTM D97 |
ExxonMobil 220 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Pour Point | -36.0 °C | -32.8 °F | ASTM D97 |
ExxonMobil 460 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Pour Point | -36.0 °C | -32.8 °F | ASTM D97 |
ExxonMobil Mobil Velocite 3 The Mobil Velocite Oil Numbered Series oils are premium performance products primarily designed for the lubrication of high-speed spindles in machine tools. They are also used in some critical hydra.. |
|||
Pour Point | <= -36.0 °C | <= -32.8 °F | |
ExxonMobil Mobilarma 525 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Pour Point | -36.0 °C | -32.8 °F | |
ChevronTexaco 32 Gas Turbine Texaco Gas Turbine oils deliver value through:Superior oxidation stability for long service life at elevated temperatures.Rust and corrosion protectionHigh viscosity index for minimum viscosity chan.. |
|||
Pour Point | -36.0 °C | -32.8 °F | ASTM D97 |
ChevronTexaco Elite-Cut® AD Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Pour Point | -36.0 °C | -32.8 °F | ASTM D97 |
ChevronTexaco HiPerSYN™ ISO 220 Oil FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation
stability, high viscosity index, high flash point, low pour point, and e.. |
|||
Pour Point | -36.0 °C | -32.8 °F | |
ChevronTexaco Regal® EP 46 Texaco Regal EP oils deliver value through:Superior oxidation stability for long service life at elevated temperatures.Rust and corrosion protectionHigh viscosity index for minimum viscosity change .. |
|||
Pour Point | -36.0 °C | -32.8 °F | ASTM D97 |
ChevronTexaco Supreme SAE 5W-30 Motor Oil FeaturesChevron Supreme Motor Oils are premium quality automotive engine oils.Chevron Supreme Motor Oils SAE 5W-20, 5W-30, 10W-30, 10W-40, and 20W-50 are formulated with ISO-SYN™ base stocks, a she.. |
|||
Pour Point | <= -36.0 °C | <= -32.8 °F | ASTM D97 |
ExxonMobil 220 Mobil SHC PM Series Mobil SHC PM Series products are supreme performance synthetic lubricants specifically designed for the most demanding industrial paper machine circulating systems. They are engineered to provide ex.. |
|||
Pour Point | -36.0 °C | -32.8 °F | |
ExxonMobil Mobil Clean 10W-30 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Pour Point | -36.0 °C | -32.8 °F | |
ExxonMobil Mobil Clean 10W-40 5000 Mobil Clean 5000 is formulated from high quality base stocks combined with modern performance additives, including an advanced detergent system to provide excellent engine cleanliness at oil drain i.. |
|||
Pour Point | -36.0 °C | -32.8 °F | ASTM D97 |
ExxonMobil Mobil Delvac 80W-140 Synthetic Gear Oil Mobil Delvac Synthetic Gear Oil 75W-90 and 80W-140 are synthetic drivetrain lubricants engineered to meet the most demanding extended drain and warranty requirements. These products are designed for.. |
|||
Pour Point | <= -36.0 °C | <= -32.8 °F | ASTM D97 |
ExxonMobil Mobil Rarus 827 The Mobil Rarus 800 Series is a line of supreme performance air compressor lubricants primarily intended for the lubrication of severe duty reciprocating air compressors. They are engineered to meet.. |
|||
Pour Point | <= -36.0 °C | <= -32.8 °F | |
ExxonMobil Mobilarma 525 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Pour Point | -36.0 °C | -32.8 °F | |
ELM® SoyFluid™ Hydraulic All Season Premium Biodegradable - Biobased Hydraulic Oil Description: ELM Biotechbased SoyFluid Hydraulic All Season Oil is a biodegradable hydraulic oil formulated with the best optimized USA grown natural seed oils that surpass the lubricity of most con.. |
|||
Pour Point | -36.0 °C | -32.8 °F | ASTM D97 |
ChevronTexaco GST® EP ISO 46 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |
|||
Pour Point | -36.0 °C | -32.8 °F | ASTM D97 |
ChevronTexaco GST® ISO 32 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |
|||
Pour Point | -36.0 °C | -32.8 °F | ASTM D97 |
ChevronTexaco RPM® SAE 15W-40 Gas Engine Oil FeaturesChevron RPM Gas Engine Oils is a premium quality heavy duty multigrade gas engine oil for use in engines running on compressed natural gas (CNG), liquefied natural gas (LNG), and liquefied p.. |
|||
Pour Point | -36.0 °C | -32.8 °F | |
ExxonMobil Mobil Clean 10W-30 High Mileage Mobil Clean High Mileage is formulated from high quality base stocks combined with the modern performance additives, including a seal conditioner to help prevent leaks in higher mileage vehicles and.. |
|||
Pour Point | -36.0 °C | -32.8 °F | ASTM D97 |
ChevronTexaco GST® ISO 46 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |
|||
Pour Point | -36.0 °C | -32.8 °F | |
ChevronTexaco Havoline® SAE 5W-30 Motor Oil All grades of Havoline Motor Oils are formulated with high quality base stocks, a shear-stable viscosity index improver, and contain detergent, dispersant, wear control, antioxidant, corrosion inhib.. |