Thermal Properties | Metric | English | Comments |
---|---|---|---|
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ExxonMobil 32 Mobil EAL Envirosyn H Series Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ExxonMobil 632 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ExxonMobil 68 Mobil EAL Envirosyn H Series Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ExxonMobil 680 Mobil DTE FM Series Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ExxonMobil Gargoyle Arctic 234 SHC 200 Series Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt.. |
|||
Pour Point | -39.0 °C | -38.2 °F | |
ExxonMobil Mobil Clean 10W-40 High Mileage Mobil Clean High Mileage is formulated from high quality base stocks combined with the modern performance additives, including a seal conditioner to help prevent leaks in higher mileage vehicles and.. |
|||
Pour Point | -39.0 °C | -38.2 °F | |
ExxonMobil Mobil Clean 5W-30 High Mileage Mobil Clean High Mileage is formulated from high quality base stocks combined with the modern performance additives, including a seal conditioner to help prevent leaks in higher mileage vehicles and.. |
|||
Pour Point | <= -39.0 °C | <= -38.2 °F | ASTM D97 |
ExxonMobil Mobil Rarus 1024 SHC 1000 Series The Mobil Rarus SHC 1000 Series is a line of supreme performance oils primarily intended for the lubrication of severe duty rotary screw and vane air compressors. They are particularly suited for se.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ExxonMobil Mobil Zerice 15 S Oil Mobil Zerice S Oils are premium quality synthetic refrigeration compressor lubricants. Based on alkyl benzenes, which due to their nature, have superior miscibility with hydrochlorofluorocarbon (R2.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ChevronTexaco HiPerSYN™ ISO 150 Oil FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation
stability, high viscosity index, high flash point, low pour point, and e.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ChevronTexaco ISO 22 Utility Oil LVI FeaturesChevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendenc.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ChevronTexaco ISO 32 Utility Oil LVI FeaturesChevron Utility Oils LVI are general purpose lubricants. Chevron Utility Oils LVI are light-colored oils that possess excellent natural low pour points, along with low carbon-forming tendenc.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ChevronTexaco ISO 46 Industrial Oil EP FeaturesChevron Industrial Oils EP are multipurpose oils for industrial service.Chevron Industrial Oils EP are designed to help minimize wear in all types of plant lubrication and also provide long .. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ChevronTexaco Journal Bearing Oil FeaturesChevron Journal Bearing Oil is a high quality, high viscosity index, paraffinic-based lubricant. It incorporates highly effective deposit control antioxidants and rust inhibitors as well as.. |
|||
Pour Point | -39.0 °C | -38.2 °F | |
ChevronTexaco Journaltex® HD 57 Texaco Journaltex HD 57 delivers value through:Excellent lubricity characteristics imparted by the additive package minimizes friction to help prevent premature bearing failure.Good rust protection .. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ChevronTexaco MP Drive Train Fluid FeaturesChevron Drive Train Fluid - MP is a multipurpose lubricant designed for use in transmissions, wet brakes, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or TO-4M requiremen.. |
|||
Pour Point | -39.0 °C | -38.2 °F | |
ChevronTexaco Pinnacle® EP 320 Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe.. |
|||
Pour Point | -39.0 °C | -38.2 °F | |
ChevronTexaco Rando® HDZ 100 Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ChevronTexaco RPM® SAE 15W-40 Heavy Duty Motor Oil Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ChevronTexaco RPM® SAE 30 Heavy Duty Motor Oil Features: Chevron RPM Heavy Duty Motor Oils are premium quality, mixed fleet motor oils meeting the performance requirements of all four-stroke gasoline engines and all naturally aspirated, turbocha.. |
|||
Pour Point | -39.0 °C | -38.2 °F | |
ChevronTexaco URSA® SAE 30 Super Plus Texaco Ursa Super Plus oils deliver value through:Oil lasts longer between drains — Good oxidation stability protects against oil thickening during manufacturers recommended oil drain periods.Vital.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ExxonMobil Gargoyle Arctic 230 SHC 200 Series Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt.. |
|||
Pour Point | -39.0 °C | -38.2 °F | |
ExxonMobil Mobil Clean 10W-30 7500 Mobil Clean 7500 is formulated from a combination of synthetic and conventional quality base stocks combined with modern performance additives, including an advanced cleaning additive system to prov.. |
|||
Pour Point | -39.0 °C | -38.2 °F | |
ExxonMobil Mobil Clean 5W-30 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ExxonMobil Mobiltrans AST Mobiltrans AST (All Season Transmission) is an extra high performance drivetrain lubricant engineered to meet Caterpillars new TO-4 performance specifications for off-highway transmissions, drive tr.. |
|||
Pour Point | -39.0 °C | -38.2 °F | ASTM D97 |
ExxonMobil 632 Mobil SHC 600 Series Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are .. |
|||
Pour Point | <= -39.0 °C | <= -38.2 °F | ASTM D97 |
ExxonMobil Mobil Rarus 1024 SHC 1000 Series The Mobil Rarus SHC 1000 Series is a line of supreme performance oils primarily intended for the lubrication of severe duty rotary screw and vane air compressors. They are particularly suited for se.. |
|||
Pour Point | <= -39.0 °C | <= -38.2 °F | ASTM D97 |
ExxonMobil Mobil Rarus 1025 SHC 1000 Series The Mobil Rarus SHC 1000 Series is a line of supreme performance oils primarily intended for the lubrication of severe duty rotary screw and vane air compressors. They are particularly suited for se.. |
|||
Pour Point | -39.0 °C | -38.2 °F | |
ExxonMobil Mobil Clean 10W-40 High Mileage Mobil Clean High Mileage is formulated from high quality base stocks combined with the modern performance additives, including a seal conditioner to help prevent leaks in higher mileage vehicles and.. |
|||
Pour Point | -39.0 °C | -38.2 °F | |
ChevronTexaco Havoline® SAE 10W-30 Synthetic Blend Motor Oil Havoline Synthetic Blend Motor Oil is formulated with a combination of synthetic and premium quality conventional base oils and an advanced additive package.Havoline Synthetic Blend Motor Oil is rec.. |