Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 140 - 150 °C | 284 - 302 °F | Average value: 149 °C Grade Count:4 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
UL RTI, Mechanical without Impact | 125 - 150 °C | 257 - 302 °F | Average value: 140 °C Grade Count:9 |
Overview of materials for Polycarbonate, High Heat This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro.. |