Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 220 °C | 428 °F | UL 746B |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | |
Industrial Laminates/Norplex MC507U Glass Fabric Description: MC507U is a utility grade, glass fabric/silicone resin binder composite product that can be substituted for NEMA G-7, in most heating, appliance insulation and some bearing applications.. |
|||
UL RTI, Mechanical without Impact | 220 °C @Thickness 0.750 mm |
428 °F @Thickness 0.0295 in |
|
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP), 30% Glass Fiber Xydar® G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology.The moldab.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | per UL card E54153 |
Arlon 49576R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | per card E54153 |
Arlon 51570R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | File E54153 |
Arlon 51629R020 0.020" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil polyLayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production mat.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 32270R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | per UL Card E54153 |
Arlon 47576R007 0.0075" (0.190 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mate.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | per UL Card E54153 |
Arlon 47576R009 0.0095" (0.241 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured RubberSide 2: Uncured RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production material. The data sho.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 51271R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneProduct Use: Flexible heater in.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 51273R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: Polyethylene This data represents typical values for the production materia.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 51279R020 0.020" (0.508 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass This data represents typical values for the production ma.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 55271R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Interleave 2: Polyethylene Product Use: Flexible heater in.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 55272R024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 55272R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 55273R060 0.060" (1.52 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, .. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 55276B028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data represents typical values for the production mate.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 55279R055 0.055" (1.40 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | per UL card E54153 |
Arlon 55570R033 0.033" (0.838 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | per UL card E54153 |
Arlon 55571R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 48981R010 0.0100" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 3 mil PolyethyleneSide 1: Uncured RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 3 mil PolyethyleneThis data represents typic.. |
|||
UL RTI, Mechanical without Impact | 220 °C | 428 °F | E54153 |
Arlon 55279R031 0.031" (0.787 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |