Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 10.0 °C | 50.0 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding MR200 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
UL RTI, Mechanical with Impact | 10.0 °C | 50.0 °F | UL 746 |
PolyOne Geon™ Vinyl Rigid Molding MR201 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
UL RTI, Mechanical with Impact | 10.0 - 85.0 °C | 50.0 - 185 °F | Average value: 59.7 °C Grade Count:35 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |