Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746C |
Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 103R PC (Europe-Africa-Middle East) LEXAN 103R is a high viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 103R is available in transparent, translucent and opaque colours. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 121 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small intricate parts. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 123R PC (Europe-Africa-Middle East) LEXAN 123R is a low viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 123R is available in transparent, translucent and opaque colours. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 161R PC (Europe-Africa-Middle East) LEXAN 161R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 161R is available in transparent, translucent and opaque colours. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 203RM PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 915R PC Lexan* 915R Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has a UL V0 rating with good flow and mold release properties... |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® BY2710X PC (Asia Pacific) BY2710X is a modified Polycarbonate (PC) resin. It is a non-filled, injection moldable grade with UL-94 V0 rating and is available in various opaque color options. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL1463T PC Copolymer (Asia Pacific) Lexan* EXL1463T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 C) ductility in combination with medium flow ch.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HF1110 PC General purpose grade. Good clarity, heat resistance, property retention and dimensional stability. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HP4REU PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold .. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HPX4R PC Copolymer (Asia Pacific) Medium flow specialty polycarbonate with outstanding processability, ductility and autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatib.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX2910 PC (Asia Pacific) Global grade. LEXAN LUX2910 is an injection moulding grade especially designed for manufacturing optical parts requiring superior flow properties combined with very high transmission and color stabi.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 3412R PC (Europe-Africa-Middle East) LEXAN 3412R is a high viscosity, 20% glass reinforced grade. It offers excellent flame retardancy and is especially designed for applications requiring high rigidity together with high heat. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 925AU PC (Asia Pacific) Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® 955A PC Lexan* 955A Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating. Lexan 955A resin is available in tran.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® EXL1414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1414T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HP1 PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® HPH4704 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® LUX9132C PC COPOLYMER Lexan* LUX9132C Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm, high flow capability and.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | |
Samsung Cheil Industries Infino® HN-1064 PC, Unreinforced FR PC material that is applied to other resin for mobile phone chargersInformation provided by Samsung Cheil Industries. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East) 6.5% glass reinforced, Super High Flow, flame retardant PBT. |
|||
UL RTI, Electrical | 130 °C @Thickness 1.47 mm |
266 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® G-3415R Glass Fiber Reinforced Polycarbonate Resin GF 15% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
UL RTI, Electrical | 130 °C | 266 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML144R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc.. |