Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 91.0 - 122 °C | 196 - 252 °F | Average value: 105 °C Grade Count:84 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |