Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 107 °C
158 - 225 °F
Average value: 94.4 °C Grade Count:36
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and ..
Deflection Temperature at 0.46 MPa (66 psi) 77.2 - 107 °C
171 - 225 °F
Average value: 89.5 °C Grade Count:55
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Deflection Temperature at 0.46 MPa (66 psi) 85.0 - 107 °C
185 - 225 °F
Average value: 97.1 °C Grade Count:14
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
Deflection Temperature at 0.46 MPa (66 psi) 93.3 - 107 °C
200 - 225 °F
Average value: 102 °C Grade Count:3
Overview of materials for Polypropylene w/ 50% Calcium Carbonate
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene w/ 50% Calcium Carbonate". Specific grades with calcium carbonate content between 45% and ..