Polymer Property : Deflection Temperature at 0.46 MPa (66 psi) = 45.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 45.0 °C
104 - 113 °F
ASTM D648-06
Proto3000 Objet Digital Materials™ DM_4310 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 45.0 °C
104 - 113 °F
ASTM D648-06
Proto3000 Objet Digital Materials™ DM_4410 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 45.0 °C
104 - 113 °F
ASTM D648-06
Proto3000 Objet Digital Materials™ DM_4510 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 45.0 °C
104 - 113 °F
ASTM D648-06
Proto3000 Objet Digital Materials™ DM_4710 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 45.0 °C
104 - 113 °F
ASTM D648-06
Proto3000 Objet Digital Materials™ DM_8505Gray20 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 45.0 °C
104 - 113 °F
ASTM D648-06
Proto3000 Objet Digital Materials™ DM_8505Gray25 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 45.0 °C
104 - 113 °F
ASTM D648-06
Proto3000 Objet Digital Materials™ DM_8505Gray35 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Deflection Temperature at 0.46 MPa (66 psi) 40.0 - 45.0 °C
104 - 113 °F
ASTM D648-06
Proto3000 Objet Digital Materials™ DM_8505Gray40 Rigid Opaque Prototyping Polymer
Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr..
Deflection Temperature at 0.46 MPa (66 psi) 41.0 - 45.0 °C
106 - 113 °F
Average value: 42.6 °C Grade Count:5
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..
Deflection Temperature at 0.46 MPa (66 psi) 41.0 - 45.0 °C
106 - 113 °F
Average value: 42.9 °C Grade Count:17
Overview of materials for Low Density Polyethylene (LDPE), Film Grade