Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 79.0 - 255 °C | 174 - 491 °F | Average value: 110 °C Grade Count:82 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 225 - 255 °C | 437 - 491 °F | Average value: 245 °C Grade Count:6 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 232 - 255 °C | 450 - 491 °F | Average value: 241 °C Grade Count:19 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 226 - 255 °C | 439 - 491 °F | Average value: 245 °C Grade Count:14 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |