Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 195 - 254 °C | 383 - 490 °F | Average value: 224 °C Grade Count:27 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 127 - 254 °C | 260 - 489 °F | Average value: 152 °C Grade Count:14 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 130 - 254 °C | 266 - 489 °F | Average value: 162 °C Grade Count:15 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |