Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 99.4 °C | 211 °F | Annealed, 0.125 in bars; ASTM D648 |
PolyOne Edgetek® AS-1000 Acrylonitrile Butadiene Styrene (ABS)
(discontinued **) Description/Features:UnfilledPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.4 °C | 211 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS/PBT 1000 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.4 °C | 211 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® ABS/PBT 1500 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.4 °C | 211 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PBT/ABS BK Availability: North AmericaForms: PelletsAppearance: BlackTPCI# 6722121Information provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.4 °C | 211 °F | Unannealed; ASTM D648 |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.4 °C | 211 °F | Unannealed; ASTM D648 |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.4 °C | 211 °F | ASTM D648 |
Plastics Group Polifil® RMC-10 10% Calcium Carbonate-Reinforced Polypropylene, High Impact Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 99.4 °C | 211 °F | Unannealed; ASTM D648 |
ExxonMobil AP3AW Polypropylene Impact Copolymer Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe.. |