Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 78.9 °C @Treatment Temp. 60.0 °C |
174 °F @Treatment Temp. 140 °F |
Annealed; ASTM D648 |
PolyOne Geon™ L6105 natural Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.9 °C | 174 °F | ASTM D648 |
Westlake Plastics Lennite® SD-P UHMW-PE (static dissipative) Carbon-powder filled, self-lubricating, moisture-repellent material with resistivity levels in the 10^5-10^9 range. This material has the highest impact strength, is lightweight, has excellent abra.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.9 °C | 174 °F | ISO 75-2/B |
ExxonMobil PP1304E3 Polypropylene Copolymer Product Description: A homopolymer resin designed for injection molding applications requiring excellent flow and good mechanical properties. It is designed for caps and closures, general applicati.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 78.9 °C | 174 °F | Molded and tested in accordance with ASTM D4976; ASTM D648 |
Dow UNIVAL™ DMDC-6400 NT 7 High Density Polyethylene Resin (HDPE) Excellent process-ability Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDC-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, wat.. |