Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 78.3 °C @Thickness 3.18 mm |
173 °F @Thickness 0.125 in |
Unannealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion 86110 white 1275 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |