Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 53.0 °C | 127 °F | ASTM D648 |
LyondellBasell Petrothene® NA324009 Low Density Polyethylene (Blow Molding Applications) ApplicationsPETROTHENE NA 324-009 is a low density homopolymer resin intended for blow molding applications. NA 324-009 provides good clarity, toughness and processability. Typical applications in.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 53.0 °C | 127 °F | ISO 75-1, -2 |
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 53.0 °C | 127 °F | ASTM D648-98c |
DSM Somos® 14120 Water-resistant resin for stereolithography, White DescriptionDSM Somos® 14120 is a low viscosity liquid photopolymer that produces strong, tough, water-resistant parts. Parts created with Somos® 14120 have a white, opaque appearance similar to p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 53.0 - 57.0 °C | 127 - 135 °F | UV Postcure; ASTM D648-07 |
DSM Somos® NeXt LV Grey The second member of the Somos® NeXt family, Somos® NeXt LV Grey delivers the durability and functionality, with a finer resolution of details and faster part processing. This third-generation, hi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 53.0 - 56.0 °C | 127 - 133 °F | ASTM D648-98c |
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 53.0 °C | 127 °F | ISO 75-1/-2 |
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET
(Unverified Data**) Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 53.0 - 55.0 °C | 127 - 131 °F | ASTM D648 |
3D Systems Accura® 60 Plastic for SLA® Systems Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 53.0 °C | 127 °F | ISO 75-1,-2 |
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66
(discontinued **) PA 6/66 |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 53.0 - 55.0 °C | 127 - 131 °F | ASTM D648 |
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView .. |