Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 43.0 °C | 109 °F | ASTM D648 |
DuPont™ Surlyn® 9720 Ionomer Resin, Zinc Surlyn® 9720 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 43.0 °C | 109 °F | ASTM D648 |
DuPont™ Surlyn® 9721 Ionomer Resin, Zinc Surlyn® 9721 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The amount of MAA and neutr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 43.0 °C | 109 °F | |
Arkema Group Pebax® MX 1059 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) Hardness 35 shore D Good resistance to oils. Applications: Automotive, cable...ISO data provided by the manufacturer, Arkema. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 43.0 °C | 109 °F | ASTM D648 |
Buckeye Polymers BP RPP 3012 C Polypropylene, 30% Mineral Filled Applications:Outdoor FurnitureCalcium carbonate-filled PP grades have a high impact toughness, moderate increased stiffness, and excel in high gloss applications. This material can be customized thr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 43.0 °C | 109 °F | ASTM D648-06 |
Proto3000 Objet VeroWhite FullCure830 Rapid Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 43.0 - 159 °C | 109 - 318 °F | Average value: 101 °C Grade Count:48 |
Overview of materials for Polypropylene with 30% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |