Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 266 °C @Thickness 6.35 mm |
511 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Therma-Tech™ LC-5000C TC LCP
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 266 - 280 °C | 510 - 536 °F | Average value: 270 °C Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 266 °C | 510 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PPA GF30 SL2 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE + Silicone LubricantFeatures: Lubricated and Good Wear ResistanceInformation provided b.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 266 °C | 510 °F | Unannealed; ASTM D648 |
Techmer ES Statiblend® PPS GF23 IM BK 23% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 23% Filler by WeightAdditive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 266 - 301 °C | 510 - 573 °F | Average value: 284 °C Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |