Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 3.50 - 4.20 µm/m-°C @Temperature 20.0 °C |
1.94 - 2.33 µin/in-°F @Temperature 68.0 °F |
|
Destech Silicon Carbide, Solid or Foamed Destech silicon carbide foam is produced by chemical vapor reaction (CVR), in which high temperature silicon bearing gases convert glassy, or vitreous, carbon foam to SiC. Destech SiC foam has no c.. |