Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 23.6 - 24.6 µm/m-°C @Temperature 20.0 - 300 °C |
13.1 - 13.7 µin/in-°F @Temperature 68.0 - 572 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |
|||
CTE, linear | 23.6 - 24.6 µm/m-°C @Temperature 20.0 - 200 °C |
13.1 - 13.7 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
CTE, linear | 23.6 - 24.6 µm/m-°C @Temperature 20.0 - 200 °C |
13.1 - 13.7 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S690 Aluminum Alloy, AlCu4MgAg, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
CTE, linear | 23.7 - 24.7 µm/m-°C @Temperature 20.0 - 200 °C |
13.2 - 13.7 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
CTE, linear | 23.7 - 24.7 µm/m-°C @Temperature 20.0 - 200 °C |
13.2 - 13.7 µin/in-°F @Temperature 68.0 - 392 °F |
|
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T4 High stiffness and elongation at rupture. Property data for Condition T4 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |