Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.9 - 18.9 µm/m-°C @Temperature 20.0 - 100 °C |
9.94 - 10.5 µin/in-°F @Temperature 68.0 - 212 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6 Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo.. |
|||
CTE, linear | 17.9 - 18.9 µm/m-°C @Temperature 20.0 - 100 °C |
9.94 - 10.5 µin/in-°F @Temperature 68.0 - 212 °F |
|
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all.. |