Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 9.67 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 17.4 µm/m-°C

@Temperature 0.000 - 1000 °C
9.67 µin/in-°F

@Temperature 32.0 - 1830 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 12.7 mm (1/2 in.) thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
CTE, linear 17.4 µm/m-°C

@Temperature 0.000 - 1000 °C
9.67 µin/in-°F

@Temperature 32.0 - 1830 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, 15.9 mm thick bar
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
CTE, linear 17.4 µm/m-°C

@Temperature 0.000 - 1000 °C
9.67 µin/in-°F

@Temperature 32.0 - 1830 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 1.0 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
CTE, linear 17.4 µm/m-°C

@Temperature 0.000 - 1000 °C
9.67 µin/in-°F

@Temperature 32.0 - 1830 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
CTE, linear 17.4 µm/m-°C

@Temperature 0.000 - 1000 °C
9.67 µin/in-°F

@Temperature 32.0 - 1830 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 15.9 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
CTE, linear 17.4 µm/m-°C

@Temperature 0.000 - 1000 °C
9.67 µin/in-°F

@Temperature 32.0 - 1830 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 7.9 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
CTE, linear 17.4 µm/m-°C

@Temperature 20.0 - 900 °C
9.67 µin/in-°F

@Temperature 68.0 - 1650 °F
Haynes X-750 Nickel Alloy Sheet and Strip (AMS 5598, UNS N07750)
Haynes X-750 (UNS No. N07750) alloy is an age-hardenable, nickel-base superalloy with very good strength at temperatures up to about 1600°F (870°C). It is widely used as a wrought material for..
CTE, linear 17.4 µm/m-°C

@Temperature 0.000 - 1000 °C
9.67 µin/in-°F

@Temperature 32.0 - 1830 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 3.2 mm thick sheet
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, 20% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, 20% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, 30% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, 30% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, 30% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, 40% cold reduction, 1120°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, 40% cold reduction, 1175°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, 50% cold reduction, 1010°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, 50% cold reduction, 1065°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, cold rolled and 1050°C mill-annealed sheet
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, plate after 1000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, plate after 16000 hours at 650°C (1200°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, plate after 16000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, plate after 16000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, plate after 4000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, plate after 8000 hours at 760°C (1400°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, plate after 8000 hours at 870°C (1600°F)
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, plate, as annealed at 1025°C, rapid cooled
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of ..
CTE, linear 17.4 µm/m-°C

@Temperature 20.0 - 1000 °C
9.67 µin/in-°F

@Temperature 68.0 - 1830 °F
Haynes 625SQ® Nickel Alloy Sheet
Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, 40% cold reduction, 1010°C anneal for 5 minutes
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
CTE, linear 17.4 µm/m-°C

@Temperature 25.0 - 1000 °C
9.67 µin/in-°F

@Temperature 77.0 - 1830 °F
Haynes 625 alloy, 10% cold reduction
Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of hi..
CTE, linear 17.4 µm/m-°C

@Temperature 0.000 - 1000 °C
9.67 µin/in-°F

@Temperature 32.0 - 1830 °F
Kennametal Stellite Stellite® 6B solution heat-treated at 1232°C, air cooled, 11.1 mm thick plate, aged 3 hours at 816°C
Machined with tungsten-carbide tools. Inherent wear resistance, resistant to the wearing effects of hard, sharp particles such as in screw conveyors, rock crushing rollers, tile-making machines, and..
Copyright © lookpolymers.com All Rights Reserved