Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.3 µm/m-°C @Temperature 20.0 - 100 °C |
6.30 µin/in-°F @Temperature 68.0 - 212 °F |
|
International Mold Steel NAK55 Precipitation Hardened Mold Steel Description: NAK55 is a precipitation, or age-hardened mold steel with a through hardness of approximately 40 HRc. NAK55 is ideal for use in plastic and rubber molds and other applications where imp.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 20.0 - 100 °C |
6.30 µin/in-°F @Temperature 68.0 - 212 °F |
|
International Mold Steel NAK80 Precipitation Hardened Mold Steel Description: NAK80 is a precipitation or age-hardened mold steel with a uniform through hardness of approximately 40 HRc. It is super clean, Vacuum-Arc Remelted steel with uniform grain structure, u.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 26.7 - 204 °C |
6.30 µin/in-°F @Temperature 80.0 - 400 °F |
|
International Mold Steel Premium H13 Hot Work Die and Mold Steel Description: International Mold Steel's Premium H-13 is a chromium-based, hot work die and plastic mold steel designed for increased production rates and longer tool life. It meets the restricti.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.30 µin/in-°F @Temperature 70.0 - 200 °F |
H1075 |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 427 °C |
6.30 µin/in-°F @Temperature 70.0 - 800 °F |
A |
Crucible Steel 15-5 Precipitation Hardening Stainless Steel Crucible 15-5 is a Premium Quality precipitation-hardening stainless steel which is capable of high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is a V.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.30 µin/in-°F @Temperature 70.0 - 200 °F |
H1075 |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 427 °C |
6.30 µin/in-°F @Temperature 70.0 - 800 °F |
A |
Crucible Steel 17Cr-4Ni Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a precipitation-hardening stainless steel which is capable of a high strength and hardness levels after a relatively simple heat-treatment procedure. This grade is martensitic a.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.30 µin/in-°F @Temperature 70.0 - 200 °F |
H1075 |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 427 °C |
6.30 µin/in-°F @Temperature 70.0 - 800 °F |
A |
Crucible Steel 17Cr-4Ni Super-X® Precipitation Hardening Stainless Steel Crucible 17Cr-4Ni is a version of 17CR-4Ni which has been modified to substantially improve machinability and other properties. Patented 17Cr-4Ni Super-X meets industry specifications for 17Cr-4Ni. .. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 399 °C |
6.30 µin/in-°F @Temperature 70.0 - 750 °F |
|
Crucible Steel CPM® REX® M35HCHS High Speed Steel, AISI M35 CPM REX M35HCHS is a 5% cobalt modification of M2 high speed steel used almost exclusively for hobs and other gear cutting tools where higher red hardness is required. Made by the Crucible Particle .. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 204 °C |
6.30 µin/in-°F @Temperature 70.0 - 400 °F |
|
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11 Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.30 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 399 °C |
6.30 µin/in-°F @Temperature 750 °F |
hardened to 50 HRC |
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420 Premium grade stainless tool steelStavax® ESR is characterized by: Good corrosion resistance Good polishability Good wear resistance Good machinability Good stability in hardeningApplications: Udd.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 399 °C |
6.30 µin/in-°F @Temperature 750 °F |
hardened to 62 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 10 SUPERCLEAN 3 Powder Metallurgical Cold Work Tool Steel Chromium-molybdenum-vanadium alloyed steelUddeholm Vanadis 10 is a high vanadium alloyed powder metallurgy tool steel offering a unique combination of an excellent abrasive wear resistance in combin.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature -17.8 - 281 °C |
6.30 µin/in-°F @Temperature 0.000 - 538 °F |
|
AK Steel 430 ULTRA FORM® Stainless Steel 430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 204 °C |
6.30 µin/in-°F @Temperature 70.0 - 400 °F |
|
Schmolz + Bickenbach Cryodur® 2379 (D-2) Cold Work Die Steel Description: Cryodur® 2379 is a high carbon, high chromium tool steel developed for high wear applications and Supplied in the annealed conditionCharacteristics: Excellent abrasive wear resistance;.. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 302 °C |
6.30 µin/in-°F @Temperature 70.0 - 575 °F |
|
Schmolz + Bickenbach Cryodur® 2510 (O-1) Cold Work Die Steel Description: Cyrodur ® 2510 is a single melt Extra Fine Structure (EFS) material; and Supplied in the soft annealed conditionCharacteristics: Excellent dimensional stability during heat treatment; .. |
|||
CTE, linear | 11.3 µm/m-°C @Temperature 21.1 - 399 °C |
6.30 µin/in-°F @Temperature 70.0 - 750 °F |
|
Schmolz + Bickenbach CorroPlast® Plastic Mold Steel Description: CorroPlast® is a pre-hardened, free-machining 400 series stainless steel, specifically developed for mold bases for processing plastic; and Supplied in the pre-hardened condition with .. |