Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.6 µm/m-°C @Temperature 93.0 - 260 °C |
5.89 µin/in-°F @Temperature 199 - 500 °F |
|
Latrobe LSSâ„¢ A2 Tool Steel (ASTM A2) TLS A2 tool steel is a versatile, air-hardening tool steel that is characterized by good toughness and excellent dimensional stability in heat treatment. TLS A2 is intermediate in wear resistance be.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 21.0 - 204 °C |
5.89 µin/in-°F @Temperature 69.8 - 399 °F |
|
Latrobe DuraTechâ„¢ T15 Powder Metal High Speed Steel (ASTM T15) DuraTech T15 powder metallurgy high speed steel is cobalt-bearing super high speed steel which can be heat treated to a hardness as high as 67 Rockwell C. A high volume of hard vanadium carbides pro.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 21.0 - 204 °C |
5.89 µin/in-°F @Temperature 69.8 - 399 °F |
|
Latrobe Dynavanâ„¢ ASTM T15 Super High Speed Steel DYNAVAN (T15) is a super high speed steel designed for extra-high wear resistance and superior hot hardness. These properties result from the high carbon and vanadium contents which produce numerous.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 300 °C |
5.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott OG570 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, GG385, OG590, RG610, RG6.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 300 °C |
5.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott LF5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 300 °C |
5.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott GG455 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG385, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 300 °C |
5.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott OG550 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, GG385, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 300 °C |
5.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott VG14 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 300 °C |
5.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott VG6 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 300 °C |
5.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott VG9 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 260 °C |
5.89 µin/in-°F @Temperature 68.0 - 500 °F |
|
Crucible Steel AIRKOOL® (AISI A2) Tool Steel Airkool (AISI A2) is an air-hardening medium alloy tool steel which is heat treatable to HRC 60-62. It has wear resistance intermediate between the oil hardening tool steels (O1) and the high carbon.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 21.0 - 100 °C |
5.89 µin/in-°F @Temperature 69.8 - 212 °F |
Mean |
Dura-Bar 100-70-03 Continuously Cast Ductile Iron Bar Stock ASTM A536 Continuously cast ductile iron bar stock is produced in a wide variety of sizes and shapes, including rounds, rectangles and special shape cross sections.It often is used as a direct replacement for.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 400 °C |
5.89 µin/in-°F @Temperature 752 °F |
|
Bohler-Uddeholm BÖHLER S290 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 22.0 - 93.0 °C |
5.89 µin/in-°F @Temperature 71.6 - 199 °F |
|
Carpenter Custom 450® Stainless Steel, 25 mm Bar, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 24.0 - 93.0 °C |
5.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 538°C (1000°F) Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 24.0 - 93.0 °C |
5.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 560°C Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 400 °C |
5.89 µin/in-°F @Temperature 68.0 - 752 °F |
for the hardened and tempered condition |
Assab Steels ASP 60 Cold Work Steel ASP 60 is a W-Mo-V-Co alloyed PM high speed steel characterized by:Highest wear resistanceMaximum compressive strengthGood through hardening propertiesGood toughnessGood dimensional stability on hea.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 480 °C |
5.89 µin/in-°F @Temperature 68.0 - 896 °F |
|
ATI Allegheny Ludlum Stainless Steel Type AL 436S™ Ferric Stainless Steel The AL 436S™ alloy has a body-centered cubic, ferritic microstructure at all temperatures below the melting point. Angular titanium carbo-nitiride particles occur randomly in the ferrite matrix mi.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 500 °C |
5.89 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum Type 441 Alloy Stainless Steel Allegheny Ludlum stainless Type 441 alloy is a heat resisting ferritic grades providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dual stab.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 500 °C |
5.89 µin/in-°F @Temperature 68.0 - 932 °F |
|
ATI Allegheny Ludlum Type AL 441HP™ Stainless Steel Alloy Allegheny Ludlum stainless Type AL 441HP™ alloy is a heat resisting ferritic grade providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dua.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 22.0 - 93.0 °C |
5.89 µin/in-°F @Temperature 71.6 - 199 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 22.0 - 93.0 °C |
5.89 µin/in-°F @Temperature 71.6 - 199 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H900 (Age Hardened 482°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 22.0 - 93.0 °C |
5.89 µin/in-°F @Temperature 71.6 - 199 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 24.0 - 93.0 °C |
5.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 593°C Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 24.0 - 93.0 °C |
5.89 µin/in-°F @Temperature 75.2 - 199 °F |
|
Carpenter Extendo-Die® Hot Work Die Steel, Tempered 621°C Data provided by Carpenter Technology Corporation.This steel combines extreme toughness with good red hardness in large section sizes. This alloy may also be considered for many cold work applicati.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 22.0 - 93.0 °C |
5.89 µin/in-°F @Temperature 71.6 - 199 °F |
|
Carpenter Custom 455® Stainless Steel, Annealed, 25 mm Bar Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 300 °C |
5.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott GG395 Long Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG385, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 300 °C |
5.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott RG630 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, GG3.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 20.0 - 300 °C |
5.89 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott RG780 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 10.6 µm/m-°C @Temperature 500 °C |
5.89 µin/in-°F @Temperature 932 °F |
|
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Alpha-Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, .. |