Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.20 µm/m-°C @Temperature -173 - 27.0 °C |
5.11 µin/in-°F @Temperature -279 - 80.6 °F |
|
Osprey Metals CE11 Al-Si Controlled Expansion Alloy Al-50%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 9.19 µm/m-°C @Temperature 400 °C |
5.11 µin/in-°F @Temperature 752 °F |
|
Plansee CFY Chromium-Iron-Yttrium The most typical use for CFY is as interconnects in fuel cells.Characteristics: Coefficient of expansion - designed for compatibility with that of the electrolyte in fuel cells Corrosion resistance.. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 300 °C |
5.11 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck MoCu 65/35 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 300 °C |
5.11 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck WCu 70/30 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 450 °C |
5.11 µin/in-°F @Temperature 68.0 - 842 °F |
|
H.C. Starck WCu 75/25 Tungsten-Copper Composite Material Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm.. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.11 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott WG280 Long Pass Filter Base glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG420, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG66.. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 300 °C |
5.11 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott F2 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 300 °C |
5.11 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott F2HT Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 300 °C |
5.11 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott LLF1 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.11 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-FK5 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 300 °C |
5.11 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-K5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 300 °C |
5.11 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF5 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 300 °C |
5.11 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott SF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 300 °C |
5.11 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott SF57 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 300 °C |
5.11 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott SF57HHT Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.11 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott VG14 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.11 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott VG9 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 250 °C |
5.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al), Anneal Strip/Sheet High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 250 °C |
5.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 482°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 250 °C |
5.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 100 °C |
5.11 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum Type 441 Alloy Stainless Steel Allegheny Ludlum stainless Type 441 alloy is a heat resisting ferritic grades providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dual stab.. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 20.0 - 100 °C |
5.11 µin/in-°F @Temperature 68.0 - 212 °F |
Type 441 |
ATI Allegheny Ludlum Type AL 441HP™ Stainless Steel Alloy Allegheny Ludlum stainless Type AL 441HP™ alloy is a heat resisting ferritic grade providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dua.. |
|||
CTE, linear | 9.20 µm/m-°C @Temperature 200 °C |
5.11 µin/in-°F @Temperature 392 °F |
|
Ceramic Process Systems AlSiC-9, 63 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |