Category | Ceramic , Glass |
Manufacturer | Schott North America |
Trade Name | |
Port | Shanghai port,China |
Trade Terms | FOB, CFR, CIF |
Payment Terms | L/C, T/T, Western Union |
Download PDF | Schott N-FK5 Glass.pdf ![]() |
Price | EMAIL US sales@lookpolymers.com |
Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.45 g/cc | 0.0885 lb/in³ |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Knoop Microhardness | 520 | 520 | .1/20 |
Modulus of Elasticity | 62.0 GPa | 8990 ksi | |
Poissons Ratio | 0.232 | 0.232 | |
Shear Modulus | 25.0 GPa | 3630 ksi | calculated |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.20 µm/m-°C @Temperature -30.0 - 70.0 °C |
5.11 µin/in-°F @Temperature -22.0 - 158 °F |
|
10.0 µm/m-°C @Temperature 20.0 - 300 °C |
5.56 µin/in-°F @Temperature 68.0 - 572 °F |
||
Specific Heat Capacity | 0.808 J/g-°C | 0.193 BTU/lb-°F | |
Thermal Conductivity | 0.925 W/m-K | 6.42 BTU-in/hr-ft²-°F | |
Transformation Temperature, Tg | 466 °C | 871 °F |
Optical Properties | Metric | English | Comments |
---|---|---|---|
Refractive Index | 1.48749 @Wavelength 587.6 nm |
1.48749 @Wavelength 587.6 nm |
n<sub>d</sub> |
1.48914 @Wavelength 546.1 nm |
1.48914 @Wavelength 546.1 nm |
n<sub>e</sub> | |
Transmission, Visible | 99.6 % @Thickness 10.0 mm, Wavelength 380 nm |
99.6 % @Thickness 0.394 in, Wavelength 380 nm |
|
99.7 % @Thickness 10.0 mm, Wavelength 460 nm |
99.7 % @Thickness 0.394 in, Wavelength 460 nm |
||
99.8 % @Thickness 10.0 mm, Wavelength 580 nm |
99.8 % @Thickness 0.394 in, Wavelength 580 nm |
||
99.8 % @Thickness 10.0 mm, Wavelength 700 nm |
99.8 % @Thickness 0.394 in, Wavelength 700 nm |
||
99.8 % @Thickness 10.0 mm, Wavelength 405 nm |
99.8 % @Thickness 0.394 in, Wavelength 405 nm |
||
IR Transmittance | 67.9 % @Thickness 10.0 mm, Wavelength 2500 nm |
67.9 % @Thickness 0.394 in, Wavelength 2500 nm |
|
98.6 % @Thickness 10.0 mm, Wavelength 1530 nm |
98.6 % @Thickness 0.394 in, Wavelength 1530 nm |
||
UV Transmittance | 7.0 % @Thickness 10.0 mm, Wavelength 270 nm |
7.0 % @Thickness 0.394 in, Wavelength 270 nm |
|
86.7 % @Thickness 10.0 mm, Wavelength 300 nm |
86.7 % @Thickness 0.394 in, Wavelength 300 nm |
||
98.9 % @Thickness 10.0 mm, Wavelength 334 nm |
98.9 % @Thickness 0.394 in, Wavelength 334 nm |
||
99.7 % @Thickness 10.0 mm, Wavelength 370 nm |
99.7 % @Thickness 0.394 in, Wavelength 370 nm |
Chemical Properties | Metric | English | Comments |
---|---|---|---|
Acid Class, SR | 4.0 | 4.0 | |
Alkali Class, AR | 2.0 | 2.0 | |
Stain Resistance Class, FR | 1.0 | 1.0 |
Descriptive Properties | Value | Comments |
---|---|---|
B | 1 | |
Climatic Resistance Test CR | 2 | |
HG | 3 | |
K (10-6mm2/N) | 2.91 | |
Phosphate Resistance PR | 2.3 | |
T1013.0 (°C) | 469 | |
T107.6 (°C) | 672 |