Thermal Properties Metric English Comments
CTE, linear 9.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
5.06 µin/in-°F

@Temperature -22.0 - 158 °F
Schott LF5 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 9.10 µm/m-°C

@Temperature 20.0 - 300 °C
5.06 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-F2 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 9.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
5.06 µin/in-°F

@Temperature -22.0 - 158 °F
Schott N-SF1 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 9.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
5.06 µin/in-°F

@Temperature -22.0 - 158 °F
Schott VG6 Band Pass Filter
Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.
CTE, linear 9.10 µm/m-°C

@Temperature 20.0 - 300 °C
5.06 µin/in-°F

@Temperature 68.0 - 572 °F
Schott N-LAF2 Glass
Information Provided by SCHOTT North America, Inc.
CTE, linear 9.10 µm/m-°C

@Temperature 30.0 - 150 °C
5.06 µin/in-°F

@Temperature 86.0 - 302 °F
Ametek Molybdenum-Copper Composite AMC 6436
Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng..
CTE, linear 9.10 µm/m-°C

@Temperature -30.0 - 70.0 °C
5.06 µin/in-°F

@Temperature -22.0 - 158 °F